Research Article

[Retracted] Optimization of the Spark Plasma Sintering Process for High-Volume Fraction Tungsten Carbide/Al 2025 Composites

Table 3

Calculation indices of the L9 orthogonal array.

Orthogonal arrayABC

Density
K112.942.902.85
K122.912.902.92
K132.882.912.93
R0.030.020.06
Level of optimumA2B3C3

Bending strength
K11709.1709.26632.42
K12716.12692.42732.87
K13658.18691.27726.34
R51.8322.9493.62
Level of optimumA2B1C2