Research Article

Effect of TaC/Ti/Si3N4 Hard Ceramics on Mechanical and Microstructural Behaviour of AA7075 Processed through Stir Casting Process

Figure 10

EDAX pattern of (a) AA7075 and (b) AA7075 + 1wt%TaC + 8wt%Si3N4 + 0.5wt%Ti.
(a)
(b)