Control factors – stir casting process.

S. No.Processing conditionsValues

1Time for stirring5 minutes
2Stirring speed200 rpm
3Temperature of melt650°C
4Temperature during stirring670 to 700°C
4Preheating temperature250 to 300°C
5Crucible size/company4/bell
6Maximum temperature of the furnace750°C
7Type of furnaceElectric muffle furnace
8Mould size100 × 100 × 10 mm3