Research Article
Catalytic and Photocatalytic Degradation Activities of Nanoscale Mn-Doped ZnCr2O4
Table 1
BET surface area, average pore diameter, pore volume, and their crystallite size (nm) of pristine and Mn-doped ZnCr2O4 samples.
| Catalyst properties | ZnCr2O4 | Zn0.99Mn0.01Cr2O4 | Zn0.98Mn0.02Cr2O4 | Zn0.97Mn0.03Cr2O4 |
| SBET (m2/g) | 37.87 | 44.87 | 49.99954 | 53.54 | Rp (Å) | 20.20 | 16.33 | 12.23 | 15.89 | Vp (cm3/g) | 0.0731 | 0.0890 | 0.1098 | 0.0993 | Crystallite size (nm) | 29.68 | 27.34 | 22.45 | 20.80 |
|
|