Research Article
The Effect of Additive ZRJ-S1 on Mechanical Properties of Portland Cement
Table 6
Mechanical parameters of cycle peak (ZRJ-S1 (0.05 wt%) reinforced).
| Cycle sample | Cycle no. | Loading | Unloading | Poisson ratio | Elastic modulus (MPa) | Poisson ratio | Elastic modulus (MPa) |
| ZRJ-S1 (0.05 wt%) reinforced | 1 | 0.406 | 8625.2 | 0.227 | 2028.4 | 2 | 0.256 | 1993.9 | 0.224 | 1436.4 | 3 | 0.261 | 1469.6 | 0.257 | 1206.4 | 4 | 0.277 | 1201.2 | 0.280 | 1023.4 | 5 | 0.297 | 1081.9 | 0.304 | 939.9 | 6 | 0.328 | 958.6 | 0.330 | 855.7 | 7 | 0.343 | 860.3 | 0.364 | 808.6 |
|
|
Note. Loading rate at 1.6 kN/min and unloading speed rate at 3.2 kN/min, test pressure of 20.7 MPa and test temperature of 119°C.
|