Technical properties of PA6.

ModifierDensity/g·cm−3Melting point (°C)Decomposition temperature (°C)Tensile strength (MPa)Bending strength (MPa)

PA61.13215>300>60.090
Balanced water absorption/%Flash point/°CFineness/mesh
3.5>40010000