NanoparticlesDensityParticle size
1 nm10 nm100 nm1 um

TiO24260244 years2.4 years9 days2.1 hours
ZnO25606192 years2 years7 days1.7 hours
SiO22430618 years6.2 years23 days5.4 hours
AI2O23950300 years3 years11 days2.6 hours
ZrO258900181 years1.8 years6.6 days1.6 hours