Research Article

Potential Assessment of E-Waste Plastic in Metakaolin Based Geopolymer Using Petrography Image Analysis

Table 10

Split tensile strength test of mix with 10M solution at 28 days.

S. No.Binder ratio1 : 2.51 : 3

180% MK + 20% FA2.862.99
270% MK + 30% FA3.153.14
360% MK + 40% FA3.594.03
450% MK + 50% FA3.223.37