Flexural strength test of mix with 8M solution at 28 days.
| S. No. | Binder ratio | 1 : 2.5 | 1 : 3 |
| 1 | 80% MK + 20% FA | 2.75 | 3.17 | 2 | 70% MK + 30% FA | 3.08 | 4.02 | 3 | 60% MK + 40% FA | 3.47 | 4.37 | 4 | 50% MK + 50% FA | 3.19 | 3.82 |
|
|