Potential Assessment of E-Waste Plastic in Metakaolin Based Geopolymer Using Petrography Image Analysis
Table 12
Flexural strength test of mix with 10M solution at 28 days.
| S. No. | Binder ratio | 1 : 2.5 | 1 : 3 |
| 1 | 80% MK + 20% FA | 3.11 | 3.17 | 2 | 70% MK + 30% FA | 3.13 | 4.06 | 3 | 60% MK + 40% FA | 3.69 | 3.16 | 4 | 50% MK + 50% FA | 3.36 | 3.77 |
|
|