Compressive strength test for different of % EWP.

MixPercentage of EWP as replacement of crushed Agg.3rd day (N/mm2)7th day (N/mm2)28th day (N/mm2)% Drop

MC15018.3729.3936.74—
MC15-5518.2729.2336.540.544
MC15-101015.0624.1030.1218.02
MC15-151514.1622.6628.3222.92