Split tensile strength test for different of % EWP.
| Mix | Percentage of EWP as replacement of crushed Agg. | 3rd day (N/mm2) | 7th day (N/mm2) | 28th day (N/mm2) | % Drop |
| MC15 | 0 | 1.56 | 2.50 | 3.12 | ā | MC15-5 | 5 | 1.46 | 2.34 | 2.92 | 06.10 | MC15-10 | 10 | 1.31 | 2.10 | 2.62 | 16.09 | MC15-15 | 15 | 1.18 | 1.88 | 2.35 | 24.73 |
|
|