Research Article
Potential Assessment of E-Waste Plastic in Metakaolin Based Geopolymer Using Petrography Image Analysis
Table 15
Flexural strength test for different of % EWP.
| Mix | Percentage of EWP as replacement of crushed Agg. | 3rd day (N/mm2) | 7th day (N/mm2) | 28th day (N/mm2) | % Drop |
| MC15 | 0 | 2.02 | 3.23 | 4.04 | ā | MC15-5 | 5 | 1.74 | 2.78 | 3.47 | 14.11 | MC15-10 | 10 | 1.58 | 2.53 | 3.16 | 21.74 | MC15-15 | 15 | 1.39 | 2.22 | 2.78 | 31.33 |
|
|