Research Article

Potential Assessment of E-Waste Plastic in Metakaolin Based Geopolymer Using Petrography Image Analysis

Table 4

Cube crushing strength test of mix with 8 M solution (1 : 2.5).

MixBinder ratio7th day (N/mm2)28th day (N/mm2)

MC180% MK + 20% FA29.1129.69
MC270% MK + 30% FA29.8130.88
MC360% MK + 40% FA32.2132.97