Structure and Mechanical Properties of Titanium Processed by Twist Extrusion and Subsequent Rolling
Figure 10
The workpiece microstructure after the TE and the second stage of rolling (h = 2.5 mm, heating 350°C): (a) rolling after the TE; (b) rolling of the extreme part of the sample without complete processing by the TE.