Research Article
Structure and Mechanical Properties of Titanium Processed by Twist Extrusion and Subsequent Rolling
Figure 11
The shape of the samples: (a) after the second stage of deformation (dimensions: 2.5 × 17 × 50 mm); after the third stage according to the TE and rolling mode: (b) at an initial temperature of 340°C, rolling in 3 passes (8%, 13%, and 19%), h = 1.6 mm; (c) at an initial temperature of 385°С, rolling in 2 passes (40% and 20%), h = 1.2 mm.
(a) |
(b) |
(c) |