Research Article
Structure and Mechanical Properties of Titanium Processed by Twist Extrusion and Subsequent Rolling
Figure 14
Microstructure in the area of crystallite boundaries in the sample after the TE and the second stage of rolling (h = 2.5 mm, heating 350°C): (a) crystallite boundary fragment in the sample; (b) FFT processing of the selected area.
(a) |
(b) |