Structure and Mechanical Properties of Titanium Processed by Twist Extrusion and Subsequent Rolling
Figure 16
Fracture surface of rolled samples after tensile testing at 20°C: (a) after the first stage of processing (h = 1.6 mm); (b) after the second stage of processing (h = 2.5 mm).