Research Article

Structure and Mechanical Properties of Titanium Processed by Twist Extrusion and Subsequent Rolling

Figure 17

Tensile results of samples obtained after SPD processing by the TE method (e = 4.6) and rolling in the temperature range of 350–200°C: 0 indicates after the TE; 1 indicates after the 1st stage of rolling (e = 0.91); 2 indicates after the 2nd stage of rolling (e = 2.19); 3 indicates after the 3rd stage of cross rolling at 385°С (e = 3).