Research Article

Mechanical Behaviors and Damage Evolution Characteristics of Predamaged Rock under Triaxial Compression Experiment

Table 1

Predamaged degree of a rock sample.

SampleNumber of cyclesAccumulated AE ring countsPredamaged degree/D0

S-00.00.00.0
S-17.014.00.1
S-210.019.80.2
S-313.032.20.4
S-416.061.10.7
S-519.082.61.0