Research Article
Research on Rejuvenation of Styrene-Butadiene-Styrene Block Copolymer Modified Asphalt with Rejuvenating Agent Based on Pre-Mixing Method
Table 8
Effect of rejuvenating agent content on regenerated asphalt.
| Rejuvenating agentcontent, % | Ductility at 5°C, cm | Rotation viscosity, Pa.s | Penetration, 0.1 mm | Softening point, °C | 135°C | 163°C | 15°C | 25°C | 30°C |
| 0 | 4.6 | 3.451 | 0.682 | 20.6 | 39.5 | 65.7 | 72.6 | 4 | 24.9 | 2.765 | 0.583 | 22.7 | 50.3 | 75.2 | 59.0 | 8 | 32.4 | 2.016 | 0.433 | 30.5 | 69.3 | 92.9 | 55.7 | 12 | 34.5 | 1.534 | 0.353 | 36.4 | 78.1 | 122.6 | 54.6 | 16 | 35.8 | 1.224 | 0.273 | 45.9 | 108.1 | 160.1 | 44.7 | 100 | — | 0.727 | — | — | — | — | — |
|
|