Research Article
Wire Electrical Discharge Machining Characteristics of Al-4.4 Mg-0.7 Mn-0.15 Cr-12 wt.% MoO3 Composites Using Taguchi Technique
Table 3
Mean of SN ratios for the MRR and SR.
| | MRR | | Level | TON (μs) | TOFF (μs) | I (A) |
| | 1 | −21.23 | −25.43 | −21.14 | | 2 | −19.42 | −18.08 | −24.73 | | 3 | −22.81 | −18.32 | −18.78 | | 4 | −22.53 | −24.17 | −21.35 | | Delta | 3.39 | 7.35 | 5.95 | | Rank | 3 | 1 | 2 |
| | SR | | Level | TON (μs) | TOFF (μs) | I (A) |
| | 1 | −9.013 | −5.360 | −8.737 | | 2 | −9.212 | −10.632 | −8.828 | | 3 | −7.489 | −10.561 | −8.738 | | 4 | −9.666 | −8.826 | −9.076 | | Delta | 2.178 | 5.273 | 0.339 | | Rank | 2 | 1 | 3 |
|
|