Physical properties after aging.
| Asphalt type | L T (%) | K P (%) | ∆T (°C) | Ductility (cm) | Rate of change of ductility (%) |
| SBS/PTW high-viscosity-modified asphalt | −0.01 | 88.8 | 1.06 | 27.4 | 31.8 | HMA-I | −0.01 | 81.4 | 1.71 | 33.5 | 33.1 | HMA-II | −0.2 | 71.7 | 2.45 | 34.9 | 36.3 | HMA-III | −0.04 | 65.2 | 3.08 | 19.4 | 46.8 |
|
|