Research Article
Influence of End Milling Process Variables on Material Removal Rate and Surface Roughness of Direct Metal Laser Sintered Inconel 718 Plate
Table 1
Parameters for fabricating Inconel 718 plate.
| Parameter | Value |
| Layer thickness | 100 microns | Scan speed | 7.0 m/s | Powder particles | 20 microns | Build direction | Vertical | Laser power | 2000 W | Platform preheat | 80°C | Part orientation | 15°C inclined vertical | Recoating speed | 100 mm/s |
|
|