Research Article
Effect of Salt Solution on the Mechanical Behaviours of Geopolymer Concrete under Dry-Wet Cycles
Table 1
The orthogonal experimental design.
| Numbers | Fly ash | solution | solution | Cement |
| OT1 | 200 | 35.3 | 72.5 | 20 |
| OT2 | 200 | 45.7 | 90.8 | 20 |
| OT3 | 200 | 48.6 | 114.3 | 20 |
| OT4 | 400 | 35.3 | 90.8 | 20 |
| OT5 | 400 | 45.7 | 114.3 | 20 |
| OT6 | 400 | 48.6 | 72.5 | 20 |
| OT7 | 600 | 35.3 | 114.3 | 20 |
| OT8 | 600 | 45.7 | 72.5 | 20 |
| OT9 | 600 | 48.6 | 90.8 | 20 |
|
|