Research Article
Metallographic Investigation on Postweld Heat-Treated0.21%C-1020 Steel Plates Joined by SMAW Method
Table 3
Different parameters corresponding to tensile test.
| Properties/Specimen | Air-cooled | Water-quenched | Oil-quenched | Sand-cooled |
| Tensile strength (MPa) | 200 | 289 | 550 (175%↑ than air-cooled; 90%↑ than water-quenched; 66%↑ than sand-cooled) | 332 | Extension at tensile strength (mm) | 0.7 | 0.2 | 0.5 | 1 (43%↑ than air-cooled; 400%↑ than water-quenched; 100%↑ than oil-quenched) | Load at tensile strength (N) | 7214 | 10424 | 9013 | 11960 (66%↑ than air-cooled; 15%↑ than water-quenched; 33%↑ than oil-quenched) | Modulus of elasticity (MPa) | 57551 | 69399 (20%↑ than air-cooled; 13%↑ than oil-quenched; 22%↑ than sand-cooled) | 61344 | 57024 |
|
|