Research Article
Investigations on Wear Behavior of Aluminium Composites at Elevated Temperature
| | Parameters | Value |
| | Pouring temperature | 870°C | | Preheating temperature of Al2O3 | 250°C | | Preheating temperature of mould | 250°C | | Stirring time | 7 min | | Stirring speed | 600 rpm |
|
|