Table 1
Composition of gases from HDPE polymers during catalytic pyrolysis at 450°C (weight % on polymers) [
7].
| | Gases | Wt.% on polymer |
| | Hydrogen H2 | 0.00 | | Carbon dioxide CO2 | 0.00 | | Carbon monoxide CO | 0.00 | | Methane CH4 | 0.01 | | Ethane C2H6 | 0.01 | | Ethylene C2H4 | 0.02 | | Propane C3H8 | 0.05 | | Propylene C3H6 | 0.44 | | nC4 | 1.25 | | nC5 | 0.37 | | iC5 | 0.69 | | C6 | 0.44 | | Total | 3.28 |
|
|