Research Article

Effect of Boron Carbide Particles Addition on the Mechanical and Wear Behavior of Aluminium Alloy Composites

Figure 14

Worn surface SEM micrographs of (a) Al7049 alloy, (b) Al7049 with 3 wt.% B4C, (c) Al7049 with 6 wt.% B4C, and (d) Al7049 with 9 wt.% B4C composites at 4 kg load and 400 rpm speed.
(a)
(b)
(c)
(d)