Research Article

Experimental Investigations of Nano Finishing Process on Nickel-Free Austenitic Stainless Steel by Grey Relational and Principal Component Analysis

Table 5

Analysis of variance.

SourceDFSeqSSAdj SSAdj MSF% Count

Pressure (bar)20.00340.00340.00173.520.051.78
Current (A)20.13350.13350.0668139.5≤0.00170.7
NOC20.04220.04230.021244.22≤0.00122.4
Error200.00960.00950.00055.06
Total260.1888

S = 0.0218703 R-Sq = 94.93% R-Sq (adj) = 93.41%.