Research Article
Forging Temperature Effects on Crack Tip Creep Behaviour of Hot Hammer Forged Ti-6Al-4V Alloy
Figure 8
Equivalent creep strain (CEEQ) distribution of Ti-6Al-4V alloy in the crack tip region at different forging temperatures: (1#) 925°C, (2#) 975°C, (3#) 950°C, and (4#) 1000°C.