Study on the Influence of SAP on Properties of White Fair-Faced Concrete with Limestone Powder
Table 2
Mixing ratio of fair-faced concrete (kg/m3).
| Specimen number | White cement | Portland cement | Limestone powder | Fly ash | Gravel | Sand | Water | Water reducer | Super absorbent resin | Internal maintenance water |
| C | 0 | 317 | 0 | 133 | 1083 | 752 | 150 | 4.6 | 0 | 0 | AC | 158.5 | 158.5 | 0 | 133 | 1083 | 752 | 150 | 4.6 | 0 | 0 | SAC | 158.5 | 158.5 | 0 | 133 | 1083 | 752 | 150 | 4.6 | 0.9 | 9 | LSAC-10 | 136 | 136 | 45 | 133 | 1083 | 752 | 150 | 4.6 | 0.9 | 9 | LSAC-20 | 113.5 | 113.5 | 90 | 133 | 1083 | 752 | 150 | 4.6 | 0.9 | 9 | LSAC-30 | 91 | 91 | 135 | 133 | 1083 | 752 | 150 | 4.6 | 0.9 | 9 |
|
|