Comparative Study on LC3-50 with OPC Concrete Using Raw Materials from Pakistan

Table 2

Mix design of OPC and LC3-50 concrete sample considered in this study.

Materials (Kg/m3)Concrete
OPCLC3-50

Total binder370370
OPC370185
Calcined clay0120.25
Limestone055.5
Gypsum09.25
Water-binder ratio0.4160.416
Water153.2153.2
Coarse aggregate10501050
Fine aggregate780780

The coarse aggregate constituted of a 30 : 70 mixture of 10 mm aggregate and 16 mm aggregates.