With L25 orthogonal array, the input and output factors of abrasive wear.
| S. No | Composite wt % | Granular size (μm) | Flow rate (g/min) | Velocity (m/min) | Time (s) | Mass loss (g) |
| 1 | 0 | 25 | 10 | 200 | 25 | 0.02148 | 2 | 0 | 50 | 15 | 250 | 50 | 0.02607 | 3 | 0 | 75 | 20 | 300 | 75 | 0.03128 | 4 | 0 | 100 | 25 | 350 | 100 | 0.04542 | 5 | 0 | 125 | 30 | 400 | 125 | 0.04502 | 6 | 3 | 25 | 10 | 300 | 100 | 0.01824 | 7 | 3 | 50 | 15 | 350 | 125 | 0.01916 | 8 | 3 | 75 | 20 | 400 | 25 | 0.01824 | 9 | 3 | 100 | 25 | 200 | 50 | 0.01608 | 10 | 3 | 125 | 30 | 250 | 75 | 0.017238 | 11 | 6 | 25 | 10 | 400 | 50 | 0.01357 | 12 | 6 | 50 | 15 | 200 | 75 | 0.01114 | 13 | 6 | 75 | 20 | 250 | 100 | 0.01228 | 14 | 6 | 100 | 25 | 300 | 125 | 0.01268 | 15 | 6 | 125 | 30 | 350 | 25 | 0.01140 | 16 | 9 | 25 | 10 | 250 | 125 | 0.01050 | 17 | 9 | 50 | 15 | 300 | 25 | 0.00750 | 18 | 9 | 75 | 20 | 350 | 50 | 0.00105 | 19 | 9 | 100 | 25 | 400 | 75 | 0.00464 | 20 | 9 | 125 | 30 | 200 | 100 | 0.00458 | 21 | 12 | 25 | 10 | 350 | 75 | 0.00345 | 22 | 12 | 50 | 15 | 400 | 100 | 0.00468 | 23 | 12 | 75 | 20 | 200 | 125 | 0.00348 | 24 | 12 | 100 | 25 | 250 | 25 | 0.00367 | 25 | 12 | 125 | 30 | 300 | 50 | 0.00442 |
|
|