Corrosion probe’s location along the water circuit.
| | 
 |  | Probe number | Distance from the steel unit along the water flow (m) | Relative distance from the steel unit along the water flow (%) | Distance to magnesium anode (m) |  | 
 |  | Probe 2 | 0.2 | 5 | 0.2 (outlet of steel unit) |  | Probe 3 | 1.0 | 25 | 1.0 |  | Probe 5 | 2.0 | 50 | 2.0 |  | Probe 4 | 3.0 | 75 | 1.0 |  | Probe 1 | 3.8 | 95 | 0.2 (inlet of steel unit) |  | 
 | 
 |