Research Article
Testing and Evaluation of Hard Sandstone Aggregate in Hot Mix Asphalt
Table 6
Properties of SBS-modified asphalt.
| Properties | Unit | Technical requirements | Results |
| Penetration depth at 25°C, 100 g, 5 s | 0.1 mm | 40–60 | 50 | Softening point (ring and ball method) | °C | ≥60 | 85.0 | Ductility at 5 cm/min, 5°C | cm | ≥20 | 39 | Specific relative density at 15°C | — | — | 1.060 | Rolling thin-film oven test at 163°C | | | | Weight change | % | ±1.0 | −0.105 | Retained penetration | % | ≥65 | 67 | Ductility at 5°C | cm | ≥15 | 19 |
|
|