Microstructure, Tensile Property, and Surface Quality of Glass Fiber-Reinforced Polypropylene Parts Molded by Rapid Heat Cycle Molding

Figure 4

SEM micrographs of skin layer thickness in RHCM and CIM samples produced at different cavity surface temperatures before filling: (a) CIM; (b) RHCM60; (c) RHCM90; (d) RHCM120 (unit: μm).