Research Article
Reducing the Sink Marks of a Crystalline Polymer Using External Gas-Assisted Injection Molding
Table 3
Values of the sink marks of the crystalline polymer products.
| Number | Parameter | Sink mark | (°C) | (MPa) | (mm/s) | (MPa) | (s) | (s) | (MPa) | (s) | (s) | (mm) |
| 1 | 180 | 105 | 40 | 10 | 5 | 35 | 3 | 5 | 1.5 | 0.264 | 2 | 220 | 110 | 35 | 80 | 2 | 25 | 8 | 10 | 2 | 0.155 | 3 | 220 | 70 | 60 | 90 | 3 | 10 | 1 | 30 | 1.5 | 0.0723 | 4 | 180 | 75 | 25 | 50 | 2 | 25 | 2 | 20 | 2 | 0.121 | 5 | 200 | 100 | 50 | 100 | 1 | 40 | 6 | 30 | 0.5 | 0.098 | 6 | 200 | 110 | 60 | 50 | 5 | 50 | 7 | 25 | 2 | 0.067 | 7 | 180 | 85 | 65 | 90 | 2 | 45 | 9 | 5 | 1 | 0.202 | 8 | 200 | 95 | 30 | 40 | 2 | 40 | 0 | 15 | 2.5 | 0.168 | 9 | 220 | 85 | 35 | 70 | 4 | 45 | 3 | 30 | 2.5 | 0.143 | 10 | 180 | 90 | 35 | 60 | 5 | 20 | 8 | 30 | 1 | 0.127 | 11 | 200 | 110 | 25 | 40 | 3 | 10 | 40 | 25 | 0 | 0.040 | 12 | 180 | 90 | 70 | 40 | 1 | 15 | 4 | 10 | 0.5 | 0.176 | 13 | 220 | 85 | 40 | 30 | 1 | 30 | 90 | 25 | 0 | 0.073 | 14 | 220 | 95 | 25 | 100 | 4 | 50 | 5 | 15 | 1 | 0.157 | 15 | 220 | 65 | 55 | 50 | 5 | 35 | 70 | 10 | 0 | 0.154 | 16 | 180 | 70 | 30 | 20 | 4 | 40 | 6 | 15 | 0.5 | 0.107 | 17 | 180 | 65 | 45 | 80 | 1 | 35 | 5 | 25 | 2 | 0.080 | 18 | 180 | 95 | 70 | 30 | 4 | 30 | 0 | 25 | 1.5 | 0.213 | 19 | 200 | 80 | 60 | 20 | 2 | 45 | 40 | 30 | 0 | 0.066 | 20 | 200 | 80 | 45 | 80 | 5 | 15 | 0 | 15 | 0.5 | 0.120 | 21 | 220 | 75 | 70 | 60 | 3 | 55 | 6 | 20 | 1.5 | 0.132 | 22 | 200 | 70 | 40 | 30 | 3 | 55 | 8 | 5 | 1.5 | 0.208 | 23 | 180 | 100 | 55 | 70 | 3 | 10 | 7 | 15 | 2.5 | 0.112 | 24 | 220 | 105 | 65 | 10 | 2 | 20 | 5 | 20 | 1 | 0.079 | 25 | 180 | 105 | 45 | 90 | 3 | 55 | 10 | 20 | 0 | 0.117 | 26 | 200 | 75 | 50 | 10 | 4 | 15 | 9 | 20 | 2.5 | 0.044 | 27 | 220 | 90 | 50 | 20 | 1 | 50 | 1 | 10 | 2 | 0.240 | 28 | 220 | 100 | 55 | 60 | 4 | 25 | 2 | 5 | 0.5 | 0.167 | 29 | 200 | 65 | 30 | 70 | 1 | 20 | 2 | 5 | 1 | 0.172 | 30 | 200 | 80 | 65 | 100 | 5 | 30 | 4 | 10 | 2.5 | 0.145 |
|
|