Research Article
Effect of Oxidized Wood Pulp Fibers on the Performance of the Thermoplastic Corn Starch Composites
Figure 5
SEM micrographs of the fracture surface of OWPF/TPS composites with different oxidation degrees: (a) 0.125 OWPF/TPS; (b) 0.25 OWPF/TPS; (c) 0.375 OWPF/TPS; (d) 0.5 OWPF/TPS.
| (a) |
| (b) |
| (c) |
| (d) |