Research Article

Continuous Differential Microemulsion Polymerization to Prepare Nanosized Polymer Latices in Microreactors

Figure 10

Conversion versus residence time profiles for differential microemulsion polymerization and soap-free emulsion polymerization (,  min, °C, the concentration of APS was 5 mM, and the solid content of the initial microemulsion was 5.0 wt.%).