Research Article

Effect of Sepiolite-Loaded Fe2O3 on Flame Retardancy of Waterborne Polyurethane

Table 3

Microscale combustion data of the WPU and WPU composite samples.

Sample numberHRC (J/g-K)PHRR (W/g)Tp (°C)THR (kJ/g)Percentage of char (%)

S-1470.0418.9355.227.03.1
S-2302.0269.9385.026.06.9
S-3231.0206.9412.226.37.6
S-4184.0164.2390.625.214.3