Experimental Study on Reducing the Heat of Curing Reaction of Polyurethane Polymer Grouting Material
Table 6
Proportions of low exothermic polymer grouting material (%).
| White material | Component | Pre 1 | Pre 2 | Pre 3 | Flame retardant | High-boiling point solvent | Surface active agent | Tertiary amine catalyst | Organotin catalysts | H2O | HCFC-141b | Weight proportion (%) | 10.16 | 43.96 | 5.28 | 18 | 15 | 1 | 0.2 | 0.3 | 0.1 | 6 |
| Black material | Component | Prepolymer 3 (NOC of 16.6%) | Polyphenyl polymethylene isocyanate | High-boiling point solvent | Weight proportion (%) | 45 | 50 | 5 |
|
|