Introduction to the New Copolymer of Chloroprene and Acrylonitrile with Differentiated Properties

Figure 7

Changes in (a) tensile strength and (b) elongation at break of vulcanizates of acrylonitrile-chloroprene rubber (NCR), chloroprene rubber (CR), and nitrile rubber (NBR) as a function of temperature after 72 hrs in different test oils.
(a)