Crystallinity indexes of various PALF.
| Types of pineapple leaf fiber | Crystallinity index |
| Soaked for 24 hours in water- | 74.26 | Abrasive-combed | 73.12 | Fine fiber strands | 74.42 | 1% sodium hypochlorite (2 hours) | 73.14 | 1% sodium hypochlorite (4 hours) | 71.28 |
|
|