Research Article
Metallocene Polyolefins Reinforced by Low-Entanglement UHMWPE through Interfacial Entanglements
Figure 7
(a, b) Buildup of normalized storage modulus of selected samples with time at 190°C. Half time of reentanglement and reentanglement time after shear modification: (c) terminal shear rate: 10 s-1 and (d) terminal shear rate: 18 s-1.
(a) |
(b) |
(c) |
(d) |