Research Article

Improving the Physical Properties of Nanofibers Prepared by Electrospinning from Polyvinyl Chloride and Polyacrylonitrile at Low Concentrations

Table 3

Results of XRD analysis of many calculated structural parameters such as crystallinity (%), crystalline size (nm), FWHM, reflection intensity, d-spacing (d), and peak position (2θ) of pure PAN, pure PVC, and 25 : 75 PVC: PAN nanofibers.

Samplesd (nm)Rel. int. (%)FWHMCrystalline size (nm)Crystallinity (%) in (100) rel. int.

Pure PAN17.7880.4982234.80.962861.2
19.3240.45896501.0657
21.160.419521001.8834
21.4320.4142543.30.8249
250.3558946.51.1277
26.20.3398511.70.39921

Pure PVC18.320.4838880.50.4161963.44
24.1010.368961000.57614

25 : 75 PVC: PAN17.40.5092436.11.426560.00
200.4435984.81.2526
20.9850.4229884.61.2996
21.1120.420461001.3825

Rel. int.: reflection intensity, d: d-spacing, and : peak position.