Thermo-Responsive Shape Memory Thermoplastic Elastomer Based on Natural Rubber and Ethylene Octene Copolymer Blends
Table 3
DSC parameters of EOC phase in NR/EOC blends with various ethylene content of EOC.
| Parameters | NR/EOC (EOC grades) | 8842 | 8100 | 8003 | 8480 |
| Crystallization temperature (°C) | 24.3 | 43.2 | 64.7 | 85.3 | Melting temperature (°C) | 45.8 | 65.7 | 80.5 | 101.0 | Degree of crystallinity (%) | 1.31 | 2.85 | 9.02 | 15.96 |
|
|