Research Article

Thermo-Responsive Shape Memory Thermoplastic Elastomer Based on Natural Rubber and Ethylene Octene Copolymer Blends

Table 6

The glass transition temperature at 5 Hz of NR/EOC blends with various ethylene content of EOC.

ParametersNR/EOC (EOC grades)
8842810080038480

Glass transition temperature−58.17−53.67−53.42−52.75