Thermo-Responsive Shape Memory Thermoplastic Elastomer Based on Natural Rubber and Ethylene Octene Copolymer Blends
Table 8
SM properties of recyclable NR/EOC blend having 62 wt% of ethylene content in EOC phase.
| Cycle (N) | Shape fixity efficiency (%) | Shape recovery efficiency (%) |
| 1 | 99.82 ± 0.10 | 95.95 ± 0.56 | 2 | 99.17 ± 1.46 | 89.45 ± 0.56 | 3 | 94.91 ± 0.15 | 77.34 ± 0.75 | 4 | 98.32 ± 0.35 | 69.78 ± 1.04 | 5 | 96.92 ± 0.21 | 70.31 ± 0.29 |
|
|