Research Article

Tailoring the Curing Kinetics of NBR-Based Rubber Compounds for Additive Manufacturing of Rod Seals

Figure 11

Comparison of the crosslink densities of the reference (recipe #1) and both optimized mixture vulcanizates (recipe #2 and #3), as determined by swelling in THF at 25°C for 24 hr. The number of samples each recipe was n = 3.